Basecoat BC001 Metallic And Solid Colour Basecoat / Clearcoat Finishing

Basecoat BC001 Metallic And Solid Colour Basecoat / Clearcoat Finishing

  • High Light

    Basecoat BC001

    ,

    Metallic Solid Colour Basecoat

    ,

    Clearcoat Finishing Basecoat

  • Paint System
    RATIO Aqua
  • Spreading Rate
    130 M²/l At 1 µm
  • Mixing Ratio
    2:1
  • Place of Origin
    CHINA
  • Brand Name
    Fengfan
  • Model Number
    BC-001

Basecoat BC001 Metallic And Solid Colour Basecoat / Clearcoat Finishing

Basecaot BC001 Metallic And Solid-Colour Basecoat/Clearcoat Finishing

Basecaot BC001

 

Aplication: Metallic and solid-colour basecoat/clearcoat finishing.Wet-on-wet process with CC006 Clear.

Properties: Very good hiding power, high efficiency.

Remarks: • Mixing formulas with TP005 and mixing bases are available to cover the whole range of colours

needed in automotive refinishing.

• At rather high temperatures or when refinishing large surfaces, it is possible to replaceTH04 byTH03

slow,while replacing TH03 Adjusting base by TH03 slow at the same time.

• Mixtures will keep for up to 6 months when stored in containers or cans coated inside.

• Flash-off times can be reduced significantly by using appropriate air blow equipment.

• When using white colors with high spray viscosity the mixing ratio can be changed to 100 : 80.

 

 

Paint system RATIO Aqua
  Spreading rate: 130 m²/l at 1 µm

Mixing ratio

 

Reducer

2:1

100% by vol. BC001 /Solids (acc. to mixing formula)

50% by vol. TH03 Adjusting Base *

(stir IMMEDIATELY after having added adjusting base)

*When using TH04 slow in the mixing formula, TH03 slow must also be used.

Spray viscosity

DIN 4 at 20°C

approx. 18-24 s

Gravity cup

Spraying pressure

HVLP gun: 1.3 mm

2.0-3.0 bar/ 0.7 bar at the nozzle

Compliant gravity-feed gun

1.3-1.4 mm, 2.0 bar

Number of spraycoats 2 (spray to cover) + ½ to match the effect Film thickness: 10-15 µm
Flash-off at 20°C Approx. 5 min. after each spraycoat.

Intermediate drying

Drying at 20°C

Blow dry with Dry Jet

Flash off until mat after each spraycoat.
Sanding Remove dust nibs by dry sanding; gently fade out applying mist coat afterwards.